Arkema Group Evatane® 1090 VN 3 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer Arkema
Trade Name Evatane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Evatane® 1090 VN 3 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: EVA copolymer made by high pressure tubular process.Applications:Grade for molding flexible articles.Examples: Closures, plugs, swimming flippers, toys.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.929 g/cc
0.0336 lb/in³
Melt Flow 11.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.00 MPa
725 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.0950 GPa
13.8 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
10°C/min
Vicat Softening Point 71.0 °C
160 °F
50°C/hr; 50N
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.