ArcelorMittal 51+AS Aluminized steel

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer ArcelorMittal
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ArcelorMittal 51+AS Aluminized steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Use: Roll forming - Lock seamingInformation provided by ArcelorMittal
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 270 - 500 MPa
39200 - 72500 psi
Elongation at Break >= 22 %
>= 22 %
80 mm