Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer Owens Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owens Corning.
Physical Properties Metric English Comments
Density 1.64 g/cc
0.0592 lb/in³
ASTM D792
Water Absorption 0.010 %
0.010 %
24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Ultimate 150 MPa
21800 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Modulus of Elasticity 14.1 GPa
2050 ksi
ASTM D638
Flexural Strength 260 MPa
37700 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 140 MPa
20300 psi
ASTM D695
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
V-O/5V
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+15 ohm-cm
4.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60 Hz
3.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
380 kV/in
ASTM D149
Arc Resistance 125 sec
125 sec
ASTM D495
Users viewing this material also viewed the following: