Material Notes:
High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C. Also can be used as a high temperature wire varnish/impregnant for motor stators. Available as a long pot-life, 2-component system.Information provided by Aptek Laboratories, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D1475
Viscosity 2400 cP
2400 cP
Spindle #2; speed 10 rpm; ASTM D1824
Outgassing - Total Mass Loss 0.10 %
0.10 %
Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.010 %
0.010 %
Cured property; at 10E-6 torr; ASTM E595
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Cured property; ASTM D2240
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; Perkin Elmer TMS-2
200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; Perkin Elmer TMS-2
Glass Transition Temp, Tg 165 °C
329 °F
Cured property; Perkin Elmer TMS-2
Flash Point >= 200 °C
>= 392 °F
ASTM D92
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Cured property; ASTM D257
Dielectric Constant 3.3

@Frequency 1000 Hz
3.3

@Frequency 1000 Hz
Cured property; ASTM D150
Dissipation Factor 0.0090

@Frequency 1000 Hz
0.0090

@Frequency 1000 Hz
Cured property; ASTM D150
Descriptive Properties Value Comments
Color Clear Amber