Abatron Abosolv™ General Purpose Thinner and Solvent

Category Fluid , Solvent
Manufacturer Abatron
Trade Name Abosolv™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron Abosolv™ General Purpose Thinner and Solvent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Abosolv™ is a solvent for LiquidWood®: for thinning the product and cleaning up. Abosolv™ can be added to LiquidWood® up to 1 part Abosolv™ to 1 part LiquidWood® by volume.
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc
0.870 g/cc
Density 0.00512 g/cc
0.000185 lb/in³
Vapor Density
Volatiles 100 %
100 %
Solubility in Water 0.020 %

@Temperature 25.0 °C
0.020 %

@Temperature 77.0 °F
Vapor Pressure 0.00277 bar
2.08 torr
Thermal Properties Metric English Comments
Boiling Point 159 - 170 °C
318 - 338 °F
Flash Point 42.2 °C
108 °F
Descriptive Properties Value Comments
Color Almost-colorless