ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Aerospace rings, forgings, weld wire.
Physical Properties Metric English Comments
Density 8.99 g/cc
0.325 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 94
94
Tensile Strength, Ultimate 966 MPa
140000 psi
Tensile Strength, Yield 517 MPa

@Strain 0.200 %
75000 psi

@Strain 0.200 %
Elongation at Break 50 %
50 %
Reduction of Area 50 %
50 %
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 4.0 %
4.0 %
Molybdenum, Mo 24.5 %
24.5 %
Nickel, Ni 66 %
66 %
as balance