3M Scotchfil™ Electrical Insulation Putty

Category Polymer
Manufacturer 3M
Trade Name Scotchfil™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchfil™ Electrical Insulation Putty.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotchfil™ Electrical Insulation Putty is used as a build-up compound on highly irregular surfaces such as fittings and valves, providing a smooth, waterproof taping surface. The putty is soft and pliable – simply press putty into place on irregular surfaces, mold with finger pressure and over tape using standard methods.Information provided by 3M
Physical Properties Metric English Comments
Thickness 3180 microns
125 mil
ASTM D1000
Mechanical Properties Metric English Comments
Elongation at Break >= 1000 %
>= 1000 %
ASTM D1000
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+6 ohm
>= 1.00e+6 ohm
ASTM D1000
Dielectric Strength 22.6 kV/mm
575 kV/in
ASTM D1000
Processing Properties Metric English Comments
Dry Time 0.250 hour

@Thickness 0.0254 mm
0.250 hour

@Thickness 0.00100 in
at RT at 50% RH
Descriptive Properties Value Comments
Appearance Black