Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 0.01643 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.01643 kN/m
0.09375 pli
Adhesion to Steel; ASTM D3330
3M ScotchPad™ 802 Repositionable Tape Pad
3M™ ScotchPad™ Repositionable Tape Pad 802 are pre-cut pads composed of linered sheets of low adhesion tape and can be easily applied to a surface, removed, and reapplied to another resurface. The..