3M Scotch® 893 Filament Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 893 Filament Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Tape 893 is a general-purpose packaging tape reinforced with continuous glass-yarn filaments that give the tape high tensile strength and low stretch. The clear 3M™ Scotchpro™ backing provides excellent abrasion and moisture resistance. The aggressive packaging-grade adhesive is specifically formulated to provide an excellent balance of high initial adhesion and long-term holding power to most fiberboard surfaces. When used in bundling, reinforcing, or coil tabbing applications, where high temperatures and/or oily surfaces are involved, tests should be conducted per the individual application before extensive use to determine the tape’s suitability.Information provided by 3M
Physical Properties Metric English Comments
Thickness 152 microns
6.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM D3759
Elongation at Break 4.5 %
4.5 %
ASTM D3759
Peel Strength 0.60259 kN/m
3.4375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure-sensitive rubber resin
Appearance Clear