3M Scotch® 8651 Strapping Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 8651 Strapping Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Strapping Tape is a high-performance, transparent packaging tape reinforced along its length with continuous polypropylene monofilaments, which give the tape high tensile strength. The polypropylene backing provides excellent abrasion, moisture and scuff resistance. The adhesive is a very aggressive packaging grade adhesive, specially formulated to meet the high demands of sealing corrugated fiberboard cartons, including those with high recycled content commonly used in today’s packing materials.Information provided by 3M
Physical Properties Metric English Comments
Thickness 142 microns
5.60 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 219 MPa
31700 psi
ASTM D3759
Elongation at Break 30 %
30 %
ASTM D3759
Peel Strength 0.82172 kN/m
4.6875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive synthetic rubber resin
Appearance Clear