Material Notes:
3M™ Novec™ 1710 Electronic Grade Coating is a higher solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 10 wt% fluorochemical acrylic polymer carried in a hydrofluoroether solvent.Features and Benefits:Can be used as a concentrate for maintaining coating solids concentration in application baths or incorporated with resins or other liquids for a unique solution.Easy application and processing – dries in seconds without the need for thermal post-curingContains no volatile organic compounds (VOCs) and has low global warming potentialProvides excellent repellency, anti-wetting and anti-sticking properties against liquids, water, hydrocarbons, silicones, and photoresistsInformation provided by 3M
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Solids Content 10 %
10 %
fluoropolymer
Thermal Properties Metric English Comments
Boiling Point 61.0 °C
142 °F
of Solvent
Glass Transition Temp, Tg 44.5 °C
112 °F
Optical Properties Metric English Comments
Refractive Index 1.39
1.39
Electrical Properties Metric English Comments
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
30% RH
Dielectric Strength 3.94 kV/mm
100 kV/in
35% RH
Dissipation Factor 0.0089

@Frequency 1000 Hz
0.0089

@Frequency 1000 Hz
30% RH
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
from date of manufacture in unopened container