3M Foam & Fabric 24 Spray Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Foam & Fabric
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Foam & Fabric 24 Spray Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A fast-tack industrial grade spray adhesive.Features:Fast tack adhesive bonds foam to foam, metal, wood and many other substratesIdeal for upholstery applicationsAggressive tackFoam tearing strengthInformation provided by 3M
Physical Properties Metric English Comments
Density 0.755 g/cc
0.0273 lb/in³
Solids Content 17.3 %
17.3 %
Descriptive Properties Value Comments
Appearance Orange
Base Synthetic Elastomer