3M FM04630K White Polyester Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FM04630K White Polyester Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ White Polyester Label Products FM046302 and FM04630K are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high performance tackified acrylic formulated for acid resistance and adhesion to polyolefins.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Facestock
150 microns
5.90 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.877 kN/m
5.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
150 °C
302 °F
Service
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1480 Perm. 24
Liner 83# Laser