Material Notes:
3M™ Economy Reinforced Water Activated Paper Tape 6144 is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and a high tack water activated adhesive system.Information provided by 3M
Physical Properties Metric English Comments
Thickness 124 microns
4.90 mil
Caliper; ASTM D645
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 63.3 - 70.4 MPa
9180 - 10200 psi
Film Tensile Strength at Break, TD 31.0 - 38.0 MPa
4500 - 5510 psi
Descriptive Properties Value Comments
Adhesive Type High Tack, Water Activated, modified Starch Based Adhesive