Polymer Property : Film Tensile Strength at Break, MD = 9180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 63.3 - 70.4 MPa
9180 - 10200 psi
3M 6144 Economy Reinforced Water Activated Paper Tape
3M™ Economy Reinforced Water Activated Paper Tape 6144 is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and a high tack water activat..