3M 4F94 Fire Retardant Carpet Protective Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4F94 Fire Retardant Carpet Protective Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Fire Retardant Carpet Protective Tape 4F94 is a flame retardant, thicker polyethylene tape with a very high-tack adhesive system used for temporary protection of carpets during construction or maintenance of ships and boats.Information provided by 3M
Physical Properties Metric English Comments
Thickness 114 microns
4.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 MPa
2000 psi
ASTM D882
Elongation at Break 450 %
450 %
ASTM D882
Peel Strength 0.219 kN/m
1.25 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Opaque