Material Notes:
3M™ Co-Extruded Polyethylene Protective Tape helps provide temporary protection of painted metals, glass and plastics from surface damage, such as scratching, abrading. etc.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 600 %
600 %
ASTM D882
Peel Strength 0.07669 kN/m
0.4375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Clear, blue, white