Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.80e+11 ohm-cm @Temperature 100 °C |
9.80e+11 ohm-cm @Temperature 212 °F |
IEC 672-1 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |