Polymer Property : Volume Resistivity = 8.00e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+11 ohm-cm

@Temperature 60.0 °C
8.00e+11 ohm-cm

@Temperature 140 °F
JIS-K-6723
Denka VINYKON W7080 PVC, W grade for non-migratory sheath and special items
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..