Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.00e+11 ohm-cm @Temperature 60.0 °C |
8.00e+11 ohm-cm @Temperature 140 °F |
JIS-K-6723 |
Denka VINYKON W7080 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |