Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 5.00e+7 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+7 ohm-cm

@Temperature 20.0 °C
5.00e+7 ohm-cm

@Temperature 68.0 °F
IEC 672-1
CeramTec CD 110 Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati..
Volume Resistivity 5.00e+7 ohm-cm

@Temperature 20.0 °C
5.00e+7 ohm-cm

@Temperature 68.0 °F
IEC 672-1
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat..