Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.30e+14 ohm-cm @Temperature 25.0 °C |
3.30e+14 ohm-cm @Temperature 77.0 °F |
cured 30 days @ 25°C |
Abatron AboCast/AboCure 8110-2 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |