Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+16 ohm-cm @Temperature 25.0 °C |
2.00e+16 ohm-cm @Temperature 77.0 °F |
UR324; ASTM D257 |
Lord Adhesives Thermosetâ„¢ UR312 / UR324 Urethane Encapsulating Gel UR312 A/B and UR324 A/B are the same components used at different mix ratios, therefore, giving different properties.LORD UR312 and UR324 are two-component, room temperature curing urethane gels. Th.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm @Temperature 25.0 °C |
2.00e+16 ohm-cm @Temperature 77.0 °F |
ASTM D257 |
Lord Adhesives Thermoset™ UR-322 Two Component Urethane Potting Compound Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm @Temperature 23.0 °C |
2.00e+16 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |