Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.70e+6 ohm-cm @Temperature 500 °C |
1.70e+6 ohm-cm @Temperature 932 °F |
|
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |