Polymer Property : Volume Resistivity = 1.30e+8 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+8 ohm-cm

@Temperature 250 °C
1.30e+8 ohm-cm

@Temperature 482 °F
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Volume Resistivity 1.30e+8 ohm-cm

@Temperature 350 °C
1.30e+8 ohm-cm

@Temperature 662 °F
Corning Vycor® 7950 Red Glass
Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh..