Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 0.10 ohm-cm @Temperature 500 °C |
>= 0.10 ohm-cm @Temperature 932 °F |
|
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |