Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 850 ohm-cm | <= 850 ohm-cm | Aged; CEPS-0002 |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |