Polymer Property : Volume Resistivity = 7.50e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 7.50e+15 ohm-cm
7.50e+15 ohm-cm
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 30Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..