Polymer Property : Volume Resistivity = 6.80e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 6.80e+14 ohm-cm
6.80e+14 ohm-cm
150°C for 1,000 hrs; JIS-K-6249
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over..