Volume Resistivity 6.60e+11 ohm-cm
6.60e+11 ohm-cm
ASTM D247
Plenco 4349 Phenolic, Granular, Injection Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Volume Resistivity 6.60e+11 ohm-cm
6.60e+11 ohm-cm
ASTM D247
Plenco 7100 Phenolic, Nodular, Injection Molded
PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit..
Volume Resistivity 6.60e+11 ohm-cm
6.60e+11 ohm-cm
ASTM D247
Plenco 6500 Phenolic, Briquette, Transfer Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..