Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.30e+14 ohm-cm | 6.30e+14 ohm-cm | "A" |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |