Abatron AboCast 50-11/AboCure 50-4 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 50-11/AboCure 50-4 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. AboCast 50-11/AboCure 50-4 is slow, thin, clear, room-temperature-cure epoxy system. It is characterized by the low viscosity and transparency of the AboCast component, and the variable-ratio possibilities of AboCure 50-4. This system offers the very low exotherm that is ideal for rigid and transparent encapsulation of heat sensitive components.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
AboCure 50-4
1.14 g/cc
0.0411 lb/in³
AboCast 50-11
Water Absorption 0.22 %

@Time 605000 sec
0.22 %

@Time 168 hour
Viscosity 1900 cP
1900 cP
Mechanical Properties Metric English Comments
Compressive Strength 77.2 MPa
11200 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 91.0 °C
196 °F
Deflection Temp at unknown load
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 6.30e+14 ohm-cm
6.30e+14 ohm-cm
"A"
Processing Properties Metric English Comments
Pot Life 120 - 180 min
120 - 180 min
Descriptive Properties Value Comments
Color Clear Amber
Parts by Weight (pbw) 100
AboCast 50-11
50
AboCast 50-4