Polymer Property : Volume Resistivity = 550000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 550000 - 750000 ohm-cm
550000 - 750000 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific)
Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications.