Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 220000 - 5.50e+8 ohm-cm | 220000 - 5.50e+8 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |