Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.40e+15 ohm-cm | 5.40e+15 ohm-cm | ASTM D257 |
PolyOne Geon™ Vinyl Flexible R7661A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Volume Resistivity | 5.40e+15 ohm-cm | 5.40e+15 ohm-cm | |
Momentive Performance Materials RTV5222 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |
|||
Volume Resistivity | 5.40e+15 ohm-cm | 5.40e+15 ohm-cm | |
Momentive Performance Materials RTV5223 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |
|||
Volume Resistivity | 5.40e+15 ohm-cm | 5.40e+15 ohm-cm | |
Momentive Performance Materials RTV5229 Neutral Cure, One Component RTV Adhesive Sealant RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e.. |
|||
Volume Resistivity | 5.40e+15 ohm-cm | 5.40e+15 ohm-cm | ASTM D257 |
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC) Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re.. |
|||
Volume Resistivity | 5.40e+15 ohm-cm | 5.40e+15 ohm-cm | ASTM D257 |
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa.. |