CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer CPC - Vycom Co.
Trade Name VINTEC I®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical resistance is necessary. Its high strength-to-weight ratio, cost efficiency, ease of fabrication and economic balance make it the material of choice. Vintec I conforms to ASTM D-1784-95 Class 12454-B (Formerly Type I Grade 1) and is manufactured without the use of plasticizers or fillers. It can be used in self supporting construction up to 140º F (depending on chemistry). It exhibits excellent fire ratings (UL-94V-0) and has a flame spread under 20 per ASTM-E-84. Vintec I is available in numerous colors, finishes and sizes.FEATURES AND BENEFITS Strength- Vintec I combines tensile strength and stiffness for the toughest applications. Chemical Resistance- Vintec I is resistant to most acids and alkali solutions. Workability- Vintec I can be machined, cut, welded and glued for fabrication versatility. Low Cost- Vintec I is an economical choice for fabricating equipment, tanks, pumps etc. Consistency- Vintec I is extruded through most of the available gauges for dimensional consistency. Flammability- Vintec I is self extinguishing.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Tensile Modulus 2.83 GPa
411 ksi
ASTM D638
Flexural Strength 88.3 MPa
12800 psi
Yeild; ASTM D790
Flexural Modulus 3.32 GPa
481 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 82.8 °C
181 °F
ASTM D1525
Flammability, UL94 V-0
V-0
Flame Spread Index 15
15
ASTM E84
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+15 ohm-cm
5.40e+15 ohm-cm
ASTM D257
Dielectric Constant 3.19

@Frequency 60 Hz
3.19

@Frequency 60 Hz
ASTM D150
Dielectric Strength 21.4 kV/mm
544 kV/in
ASTM D149
Dissipation Factor 0.0096

@Frequency 60 Hz
0.0096

@Frequency 60 Hz
ASTM D150
Dielectric Loss Index 0.030
0.030
ASTM D150
Descriptive Properties Value Comments
Chemical Resistance Class B
ASTM D1784
Flammability Self-Extinguishing
ASTM D635