Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+7 ohm-cm | 5.00e+7 ohm-cm | |
Zircar Refractory Composites RS-DD Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
Volume Resistivity | 1e+05 - 5.00e+7 ohm-cm | 1e+05 - 5.00e+7 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ ES-06CF-09GF/000 Polyethersulfone, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |