Material Notes:
ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory Sheet Type RS-D is available in four types: TYPE RS-DD is a rigid sheet that can be moistened with water to impart moldability.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 2.08 g/cc
0.0751 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 20.0 °C
3.89 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.250 J/g-°C
0.0598 BTU/lb-°F
Melting Point 1815 °C
3299 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Softening Point 775 °C
1430 °F
Shrinkage 1.00 - 10.0 %

@Temperature 1000 - 1500 °C
1.00 - 10.0 %

@Temperature 1830 - 2730 °F
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
SiO2 10 %
10 %
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+7 ohm-cm
5.00e+7 ohm-cm
Processing Properties Metric English Comments
Moisture Content 3.0 %
3.0 %
depending on humidity
Descriptive Properties Value Comments
Color White