Polymer Property : Volume Resistivity = 4.20e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 4.20e+12 ohm-cm
4.20e+12 ohm-cm
JIS-K-6249/ASTM D257
Fujipoly Industries Sarcon® GR-HFk Gap Filler Pad
Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak..
Volume Resistivity 4.20e+12 ohm-cm
4.20e+12 ohm-cm
JIS-K-6249/ASTM D257
Fujipoly Industries Sarcon® GR-Hk Gap Filler Pad
Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak..
Volume Resistivity 4.20e+12 ohm-cm
4.20e+12 ohm-cm
JIS-K-6249/ASTM D257
Fujipoly Industries Sarcon® GR-k Gap Filler Pad
Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak..
Volume Resistivity 4.20e+12 ohm-cm

@Temperature 50.0 °C
4.20e+12 ohm-cm

@Temperature 122 °F
ASTM D257
Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Uses Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Volume Resistivity 4.20e+12 ohm-cm

@Temperature 50.0 °C
4.20e+12 ohm-cm

@Temperature 122 °F
ASTM D257
Teknor Apex APEX® 04-A0386B-88 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex