Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C Jacket; RoHS Compliant Uses Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 72
72
10 seconds; ASTM D2240
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
Flexural Modulus 0.0752 GPa
10.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -18.0 °C
-0.400 °F
ASTM D746
Oxygen Index 36 %
36 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 4.20e+12 ohm-cm

@Temperature 50.0 °C
4.20e+12 ohm-cm

@Temperature 122 °F
ASTM D257
Descriptive Properties Value Comments
Appearance Opaque