Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.0 - 6.0 ohm-cm | 4.0 - 6.0 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Volume Resistivity | 4.0 - 6.0 ohm-cm | 4.0 - 6.0 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
Volume Resistivity | 4.0 - 6.0 ohm-cm | 4.0 - 6.0 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
Volume Resistivity | 4.0 ohm-cm @Time 540 sec |
4.0 ohm-cm @Time 0.150 hour |
25% Carbon Black |
TIMCAL ENSACO™ 260G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |