Polymer Property : Volume Resistivity = 3.70e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.70e+13 ohm-cm
3.70e+13 ohm-cm
Dow Corning HIPEC® Q3-6645 SEMICONDUCTOR PROTECTIVE COATING KIT
Two-part, transparent, low modulus LED gel encapsulant with high transparency, low viscosity, and very long working time.Information provided by Dow Corning