Dow Corning HIPEC® Q3-6645 SEMICONDUCTOR PROTECTIVE COATING KIT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Dow Corning
Trade Name HIPEC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HIPEC® Q3-6645 SEMICONDUCTOR PROTECTIVE COATING KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, transparent, low modulus LED gel encapsulant with high transparency, low viscosity, and very long working time.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 55
55
Optical Properties Metric English Comments
Refractive Index 1.394
1.394
1.402
1.402
1.393

@Wavelength 1554 nm
1.393

@Wavelength 1554 nm
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 3.70e+13 ohm-cm
3.70e+13 ohm-cm
Dielectric Constant 2.9

@Frequency 100000 Hz
2.9

@Frequency 100000 Hz
Dielectric Strength 22.6 kV/mm
574 kV/in
Dissipation Factor 0.00010

@Frequency 100000 Hz
0.00010

@Frequency 100000 Hz
Descriptive Properties Value Comments
Appearance clear
Chloride Content (%) 5E-06
Working Time (min) 960