Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.60e+11 ohm-cm | 3.60e+11 ohm-cm | ASTM D247 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Volume Resistivity | 3.60e+11 ohm-cm | 3.60e+11 ohm-cm | ASTM D247 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |