Electrical Properties Metric English Comments
Volume Resistivity 3.60e+11 ohm-cm
3.60e+11 ohm-cm
ASTM D247
Plenco 3509 Phenolic, Granular, Injection Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Volume Resistivity 3.60e+11 ohm-cm
3.60e+11 ohm-cm
ASTM D247
Plenco 2300 Phenolic, Granular, Transfer Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..