Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.50e+17 ohm-cm | 3.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Volume Resistivity | 3.50e+17 ohm-cm | 3.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL403 PC Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"". |
|||
Volume Resistivity | 3.50e+17 ohm-cm | 3.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |