Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCD915 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation materials. Flame retardant performance capable of meeting UL 1581 VW-1 require.. |
|||
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® DR51 PBT 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific) 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | GB/T1410-2006 |
Sichuan Deyang Haton® hGR40DL Polyphenylene Sulfide, Glass Fiber Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | 3.30e+16 ohm-cm | 3.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |