Electrical Properties Metric English Comments
Volume Resistivity 3.16e+11 - 3.16e+12 ohm-cm
3.16e+11 - 3.16e+12 ohm-cm
IS 3396-1979
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa..