Volume Resistivity 3.10e+14 ohm-cm
3.10e+14 ohm-cm
50% RH, 500V; ASTM D257
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer
Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe..
Volume Resistivity 3.10e+14 ohm-cm
3.10e+14 ohm-cm
50% RH; 500V; ASTM D257
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines..