Volume Resistivity 250000 ohm-cm
250000 ohm-cm
LATI Latistat 67-08 PA66, Impact Modified
Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..